Best teaches you how to eliminate the shortcomings
Author:admin / read:3037 Times / label:company news
The main reason for the under-injection is that the flow resistance is too large, which prevents the melt from continuing to flow. Factors affecting the melt flow length include: part wall thickness, mold temperature, injection pressure, melt temperature and material composition. These factors can cause short bets if n……